Sandvik Materials Technology is a developer and producer of advanced stainless steels, special alloys, titanium and other high-performance materials

Sandvik 19.13.4.L (Welding strip)

Datasheet updated 2011-10-13 13:24:16 (supersedes all previous editions)

Sandvik 19.13.4.L is a strip electrode used for the second layer to obtain corrosion resistant overlay weld deposit on a transition layer of Sandvik 22.11.L or 21.13.3.L on C-, CMn- and low-alloy steels using submerged-arc welding (SAW) with the flux Sandvik 10SW or electroslag welding (ESW) with the flux Sandvik 47S.

It gives a 317L weld deposit. There are also other possible combinations and conditions.

Standards

  • AWS EQ317L
  • EN number B 19 13 4 L

Product standards

  • EN ISO 14343
  • ASME/AWS SFA5.9

Chemical composition - strip electrode

Chemical composition, wt%
C
max
Si Mn
P
max
S
max
Cr Ni Mo Cu
max
0.02
0.4 1.5
0.020
0.020
19 14 3.6 0.3

Ferrite content

The ferrite content is nominally 7 FN WRC.

Chemical composition of overlay

Typical chemical compositions in the second layer obtained on C-Mn steel and low-alloy steel.

Chemical composition, wt%
Type of overlay
C
Cr
Ni
Mo
FN, WRC
SAW 21.13.3.L+19.13.4.L/10SW
317L, E317L
max 0,04
18-19
12,5-13,5
3,1-3,5
3-8
ESW 21.13.3.L+19.13.4.L/47S
317L, E317L
max 0,03
18-19
12,5-14
3,3-3,6
3-8
ESW 22.11.L+19.13.4.L/47S
317L, E317L
max 0,03
18-19
12,5-13,5
3,0-3,5
3-8
ESW 24.13.L+19.13.4.L/49S
E316L1), EN1.4435
max 0,03
18-19
12,5-13,5
2,5-3,0
3-8

1) minimum 2,5 % Mo
Consider the figures as examples. Parameters selected and conditions influence on the result. Please contact Sandvik for details and guidelines.

Mechanical properties of overlay

Passes side bend testing according to ASME Section IX.

Corrosion properties of overlay

Equal to the base metal 317L. The resistance to pitting corrosion better than for 316L.

Welding data

Process/Flux Size
Current, A
Voltage, V
Travel speed, mm/min
SAW/10SW 30 x 0.5 mm
300 - 425
28-30
80 - 160
SAW/10SW 60 x 0.5 mm
650 - 850
28-30
80 - 160
SAW/10SW 90 x 0.5 mm
975 - 1275
28-30
80 - 160
ESW/47S 60 x 0.5 mm
1100 - 1400
23 - 26
130 - 220
ESW/47S 90 x 0.5 mm
1650 - 2100
23 - 26
130 - 220

Direct current, with electrode positive is normally used.
The welding data in the table represent the operation capability of the flux. The desired properties of the overlay are obtained by proper selection of the settings within the ranges.

Applications

19.13.4.L is used for weld surfacing of components in the chemical, petrochemical, marine industries where corrosion resistance on par with 317L is required. Typical components are pressure vessels, heat exchangers, shafts, industrial piping etc.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Send PDF via email

Article functions

Related information

Contact us

Print this datasheet

Export to PDF

Download this datasheet as PDF or send by email.
Download as PDF

Contact us